Cement-free tiles: mix of 70% PET, 20% eggshells and 10% sand achieves the highest strength
A study published in April in the Journal of Materials Science: Polymers evaluated four mixes to make cement-free tiles from waste. The combination of 70% PET plastic, 20% crushed eggshells and 10% sand had the best mechanical strength. The pieces recorded 18.63 MPa of compressive strength, 4.10 MPa of flexural strength and 0.53% water absorption. PET replaces cement as the binder and the process does not require water curing.
In 30 seconds
- The winning mix combines 70% PET, 20% crushed eggshells and 10% sand.
- The study tested four combinations, with plastic proportions between 50% and 85%.
- The tiles reached 18.63 MPa of compressive strength and 4.10 MPa of flexural strength.
IASummary generated by artificial intelligence from a story by TN. It may contain errors: the original source prevails.



Comments
Be respectful. Comments reported by several people are hidden until a moderator reviews them.
You do not need an account to read, only to comment. Sign in with a code sent to your email or with your Google account. We only show the name you choose, never your email.